Q:- In welding procedure transfers joint tensile test the following observation were made. The specimen CSA was recorded as 40mm X 20mm and the max load applied was recorded as ____ . What is the UTS?

Posted on


(A). 237.5KN/mm^2
(B). 247.5 N/mm^2
(C). 24.5 N/mm^2
(D). 237.5 N/mm^2

Please explain how.