api 1104 cwi test questions

Q:- The exposed surfaces of each fillet-weld-break specimen shall show:

Posted on Updated on


1. No Slag inclusions greater than 1/4 inch
2. At least 3/4 inches sound metal between adjacent inclusions
3. Complete penetration and fusion
4. The tensile strength of the specimen
5. None of the above

Advertisements

Q:-When considering the advantages of site RT over UT which of the following applies?

Posted on


1. A permanent record produced, good for detecting defects which do not have significant depth in relation to axis of the X-ray beam and defect identification
2. A permanent record produced, good for detecting all surface and sub-surface defects and assessing the through thickness depths of defects
3. A permanent record produced, defect identification not so reliant on operator skill
4. No controlled areas required on site, a permanent record produced and good for assessing the extent of pipe wall thickness reductions due to internal corrosio

Q:-Lineup clamps shall be used for butt welds in accordance with the procedure specification. When it is permissible to remove the lineup clamp before the root bead is completed:

Posted on


1. The completed part of the bead shall be in approximately equal segments spaced approximately equally around the circumference of the joint. 

2. The completed part of the bead shall be removed and rewelded after removing the clamp. 

3. The completed part of the bead shall be peened before removing the clamp. 

4. The completed part of the bead shall be at least 4 inches long for all pipe sizes 